Cracking in houses: categories, causes and what to report
Almost every house has some cracks. Most are cosmetic. Some point to foundation movement, a leaking pipe or a structural problem. The trick, for inspectors and builders, is telling them apart and describing them consistently.
Last checked: 13 November 2026. This summarises the damage categories used with AS 2870; it does not reproduce the Standard. Where cracking may be structural, recommend an engineer.
Where the guidance is
- AS 2870 Residential slabs and footings, which includes an appendix classifying damage to walls and slabs by crack width and effect. It is the common reference for footing performance in houses.
- NCC Volume Two, Part H1 (structure) and Housing Provisions Section 4 (footings and slabs). See our site classification guide.
- AS 4349.1, which asks inspectors to report significant defects, including structural ones.
Damage categories for walls
AS 2870 sorts wall damage into categories by approximate crack width and what it does to the house:
| Category | Description | Approx. crack width |
|---|---|---|
| 0 | Negligible: hairline cracks | Less than 0.1 mm |
| 1 | Very slight: fine cracks that don't need repair | Less than 1 mm |
| 2 | Slight: noticeable cracks, easily filled; doors and windows stick slightly | Less than 5 mm |
| 3 | Moderate: cracks that need some opening up and patching; doors and windows stick; pipes may break | About 5 to 15 mm |
| 4 | Severe: extensive repair work, walls lean or bulge, door frames distort | About 15 to 25 mm |
The Standard expects a well-designed footing on a normal site to keep damage to the low categories. Moderate damage under abnormal moisture conditions (such as a leaking pipe or poor drainage) isn't necessarily treated as a footing failure. There is a separate classification for damage to concrete floors.
Common causes
- Reactive clay movement: seasonal wetting and drying, made worse by trees, poor drainage, leaking pipes or garden watering against the slab.
- Settlement: soft or poorly compacted fill under footings.
- Shrinkage: normal drying shrinkage in new concrete, brick and plaster, usually fine and early.
- Thermal movement: long brick walls or concrete with no articulation or control joints.
- Structural: overloading, removed walls, rotted or undersized members.
- Corrosion: rusting steel lintels or reinforcement expanding and cracking brick or concrete.
What to look at
- Width, length and pattern: stepped cracks in brickwork, diagonal cracks from window and door corners, tapered cracks (wider at one end).
- Where: around openings, at corners, over doorways, along the slab edge.
- Doors and windows that stick or have uneven gaps.
- Floors that slope or bounce.
- Signs of a cause: leaking downpipes, ponding, trees, garden beds against walls, damp patches.
- Whether it's moving: fresh, clean crack edges, recent repairs that have cracked again, or tell-tales installed to monitor it.
Writing it up
Describe the crack (location, length, approximate width, pattern), the likely category, possible causes, and what should happen next: monitor, fix the drainage, or get a structural engineer's assessment. Avoid guessing at a cause you can't support.
Sources
- Spec-Net, cracking in concrete and masonry (AS 2870 crack limits)
- ABCB Housing Provisions Section 4: ncc.abcb.gov.au
This guide is general information, not engineering advice. AS 2870 is available from Standards Australia.